Why Pots Crack (and How to Stop It)
S-cracks, rim cracks, dunting and handles popping off: the causes and the fixes.
Every pot follows the same journey, from soft clay to vitrified ceramic. Knowing the stages makes every other technique easier.
| Clay body | Typical firing | Character |
|---|---|---|
| Earthenware | Low fire, around cone 06–04 | Porous unless glazed; warm reds and buffs; great for bright colors |
| Stoneware | Mid to high fire, cone 5–10 | Dense, durable, low absorption; the workhorse for functional ware |
| Porcelain | Mid to high fire, cone 6–10 | White, can be translucent, less forgiving to throw |
Dry slowly and evenly. Uneven drying is the most common cause of cracks, especially where thick and thin sections meet.
The first firing, often to around cone 06–04, burns out organic matter and chemically bound water and turns clay into porous, durable “bisqueware” that absorbs glaze well. Fire slowly through the early stages so steam can escape.
The second firing melts the glaze into glass and matures the clay body. Ware must sit on clean shelves with an unglazed foot, because molten glaze will weld a pot to the shelf.
Clay shrinks as it dries and again as it fires, often around 10–14% in total for stoneware. Make lids, sets and fitted parts from the same clay and dry them together.
S-cracks, rim cracks, dunting and handles popping off: the causes and the fixes.
Why most potters fire twice, what temperatures to use, and when single firing makes sense.
Durable, well-fitted, properly fired glazes from safe recipes: the checklist for functional ware.